American chestnut
Castanea dentata
American chestnut measures 540 lbf on the Janka scale, about 42% as hard as northern red oak.
- It is soft and steady at once, in the lowest quarter of the list for both hardness and shrinkage across the face.
- Western hemlock and yellow-poplar have exactly the same Janka figure.
- Across all 155 woods it falls in the bottom fifth for bending strength, stiffness and radial shrinkage.
U.S. hardwoodsU.S. softwoodsImported woodsNorthern red oak
Six measures
American chestnutU.S. hardwoods medianOther woods
Bending strength
8,600 psi59.3 MPa15th weakest of 15534% below the U.S. hardwoods median4,300 psi29,900 psiStiffness
1.23 M psi8.5 GPa21st most flexible of 1550.54 M psi4.06 M psiJanka hardness
540 lbf2,402 N35th softest of 15547th of 53 U.S. hardwoods; 53% below the U.S. hardwoods median240 lbf3,680 lbfDensity
0.400.43 at 12% MC36th lightest of 1550.250.96Shrinkage across the face
6.7%radial 3.4%36th lowest of 1553.5%12.7%Cupping tendency
1.9749th highest of 1551.092.90
For its weight: strength-to-weight 21,500 psi (145th of 155).
How much it moves
Its face shrinkage of 6.7% is in the lowest quarter of the list, with an ordinary T/R ratio of 1.97.
0.40 in.
off a 6-inch flatsawn board, green to oven-dry; quartersawn 0.20 in.
- Tangential
- 6.7%
- Radial
- 3.4%
- Volume
- 11.6%
- T/R ratio
- 1.97 (107th most stable of 155)
End view, shrinkage drawn 3× life size.
Closest substitutes
- Butternut
9% softer · 10% lighter · shrinks 0.3 points less across the face
- Silver maple
30% harder · 10% heavier · shrinks 0.5 points more across the face
- Quaking aspen
35% softer · 12% lighter · same face shrinkage
Woods of similar hardness
The eight nearest on the Janka scale, lbf.
Laboratory values
Its most unusual laboratory figure is work to maximum load: 13th lowest of the 142 woods with a published value.
| Property | Green | Dry, 12% MC | Change when dried | Metric, 12% MC |
|---|---|---|---|---|
| Work to maximum load | 7.00in-lbf/in³ | 6.50in-lbf/in³ | −7% | 44.8kJ/m³ |
| Modulus of rupture | 5,600psi | 8,600psi | +54% | 59.3MPa |
| Impact bending | 24in. | 19in. | −21% | 483mm |
| Modulus of elasticity | 0.93M psi | 1.23M psi | +32% | 8.48GPa |
| Compression parallel to grain | 2,470psi | 5,320psi | +115% | 36.7MPa |
| Shear parallel to grain | 800psi | 1,080psi | +35% | 7.40MPa |
| Side hardness | 420lbf | 540lbf | +29% | 2,402N |
| Compression perpendicular | 310psi | 620psi | +100% | 4.30MPa |
| Tension perpendicular | 440psi | 460psi | +5% | 3.20MPa |
Wood Handbook Table 5-3b, Table 4-3. Data & method · Guides