Western larch
Larix occidentalis
Western larch measures 830 lbf on the Janka scale, 36% softer than northern red oak.
- Among the 37 U.S. softwoods, only longleaf pine is harder, and only Pacific silver fir shrinks more across the face.
- Drying hardens it more than most: from 510 lbf green, it gains 63% by 12% moisture, where the median wood gains 31%.
- African mahogany and American elm have exactly the same Janka figure.
U.S. hardwoodsU.S. softwoodsImported woodsNorthern red oak
Six measures
Western larchU.S. softwoods medianOther woods
Shrinkage across the face
9.1%radial 4.5%41st highest of 15528% above the U.S. softwoods median3.5%12.7%Cupping tendency
2.0243rd highest of 1551.092.90Stiffness
1.87 M psi12.9 GPa52nd stiffest of 1550.54 M psi4.06 M psiJanka hardness
830 lbf3,692 N65th softest of 1552nd of 37 U.S. softwoods; 66% above the U.S. softwoods median240 lbf3,680 lbfDensity
0.480.52 at 12% MC71st lightest of 15526% above the U.S. softwoods median0.250.96Bending strength
13,000 psi89.6 MPa75th strongest of 15528% above the U.S. softwoods median4,300 psi29,900 psi
How much it moves
Both its face shrinkage (9.1%) and its T/R ratio (2.02) sit in the middle half of the list.
0.55 in.
off a 6-inch flatsawn board, green to oven-dry; quartersawn 0.27 in.
- Tangential
- 9.1%
- Radial
- 4.5%
- Volume
- 14.0%
- T/R ratio
- 2.02 (112th most stable of 155)
End view, shrinkage drawn 3× life size.
Closest substitutes
- Shortleaf pine
17% softer · 2% lighter · shrinks 1.4 points less across the face
- Parana-pine
6% softer · 4% lighter · shrinks 1.2 points less across the face
- Douglas-fir (Coast)
14% softer · 6% lighter · shrinks 1.5 points less across the face
Woods of similar hardness
The eight nearest on the Janka scale, lbf.
Laboratory values
| Property | Green | Dry, 12% MC | Change when dried | Metric, 12% MC |
|---|---|---|---|---|
| Compression perpendicular | 400psi | 930psi | +132% | 6.40MPa |
| Impact bending | 29in. | 35in. | +21% | 889mm |
| Modulus of elasticity | 1.46M psi | 1.87M psi | +28% | 12.9GPa |
| Compression parallel to grain | 3,760psi | 7,620psi | +103% | 52.5MPa |
| Shear parallel to grain | 870psi | 1,360psi | +56% | 9.40MPa |
| Tension perpendicular | 330psi | 430psi | +30% | 3.00MPa |
| Side hardness | 510lbf | 830lbf | +63% | 3,692N |
| Work to maximum load | 10.3in-lbf/in³ | 12.6in-lbf/in³ | +22% | 86.9kJ/m³ |
| Modulus of rupture | 7,700psi | 13,000psi | +69% | 89.6MPa |
Wood Handbook Table 5-3b, Table 4-3. Data & method · Guides