Honeylocust
Gleditsia triacanthos
Honeylocust measures 1,580 lbf on the Janka scale, 22% harder than northern red oak.
- Among the 53 U.S. hardwoods, only butternut shrinks less across the face.
- It pairs hardness with little movement: harder than 78% of the woods, yet in the lowest quarter for shrinkage across the face.
- On the Janka scale its nearest neighbours are afrormosia at 1,560 lbf and peroba de campos at 1,600 lbf.
U.S. hardwoodsU.S. softwoodsImported woodsNorthern red oak
Six measures
HoneylocustU.S. hardwoods medianOther woods
Shrinkage across the face
6.6%radial 4.2%32nd lowest of 15526% below the U.S. hardwoods median3.5%12.7%Janka hardness
1,580 lbf7,028 N35th hardest of 1556th of 53 U.S. hardwoods; 36% above the U.S. hardwoods median240 lbf3,680 lbfCupping tendency
1.5735th lowest of 1551.092.90Density
0.6039th heaviest of 1550.250.96Bending strength
14,700 psi101.4 MPa54th strongest of 1554,300 psi29,900 psiStiffness
1.63 M psi11.2 GPa74th most flexible of 1550.54 M psi4.06 M psi
For its weight: stiffness-to-weight 2.72 (140th of 155).
How much it moves
Little movement, and evenly split between the two directions: one of the steadiest woods in the tables.
0.40 in.
off a 6-inch flatsawn board, green to oven-dry; quartersawn 0.25 in.
- Tangential
- 6.6%
- Radial
- 4.2%
- Volume
- 10.8%
- T/R ratio
- 1.57 (35th most stable of 155)
End view, shrinkage drawn 3× life size.
Closest substitutes
- Peroba de campos
1% harder · 3% heavier · same face shrinkage
- Sapele
4% softer · 8% lighter · shrinks 0.8 points more across the face
- Green ash
24% softer · 12% lighter · shrinks 0.5 points more across the face
Woods of similar hardness
The eight nearest on the Janka scale, lbf.
Laboratory values
Its most unusual laboratory figure is crushing strength across the grain: 2nd highest of the 90 woods with a published value.
| Property | Green | Dry, 12% MC | Change when dried | Metric, 12% MC |
|---|---|---|---|---|
| Compression perpendicular | 1,150psi | 1,840psi | +60% | 12.7MPa |
| Impact bending | 47in. | 47in. | ±0% | 1,194mm |
| Shear parallel to grain | 1,660psi | 2,250psi | +36% | 15.5MPa |
| Tension perpendicular | 930psi | 900psi | −3% | 6.20MPa |
| Side hardness | 1,390lbf | 1,580lbf | +14% | 7,028N |
| Modulus of rupture | 10,200psi | 14,700psi | +44% | 101.4MPa |
| Compression parallel to grain | 4,420psi | 7,500psi | +70% | 51.7MPa |
| Work to maximum load | 12.6in-lbf/in³ | 13.3in-lbf/in³ | +6% | 91.7kJ/m³ |
| Modulus of elasticity | 1.29M psi | 1.63M psi | +26% | 11.2GPa |
Wood Handbook Table 5-3b, Table 4-3. Data & method · Guides