Cativo
Prioria copaifera
Cativo measures 630 lbf on the Janka scale, about 49% as hard as northern red oak.
- Of the 155 woods, only four shrink less through the thickness and nine bend more easily.
- Its bending strength is 48% below the median for imported woods.
- Port-Orford-cedar has exactly the same Janka figure.
U.S. hardwoodsU.S. softwoodsImported woodsNorthern red oak
Six measures
CativoImported woods medianOther woods
Stiffness
1.11 M psi7.7 GPa10th most flexible of 15544% below the imported woods median0.54 M psi4.06 M psiShrinkage across the face
5.3%radial 2.4%14th lowest of 15533% below the imported woods median3.5%12.7%Bending strength
8,600 psi59.3 MPa15th weakest of 15548% below the imported woods median4,300 psi29,900 psiCupping tendency
2.2123rd highest of 15527% above the imported woods median1.092.90Density
0.4036th lightest of 15534% below the imported woods median0.250.96Janka hardness
630 lbf2,802 N47th softest of 15555th of 65 imported woods; 52% below the imported woods median240 lbf3,680 lbf
For its weight: stiffness-to-weight 2.77 (136th of 155); strength-to-weight 21,500 psi (145th of 155).
How much it moves
Total movement is small, but most of it runs along the rings (T/R 2.21), so a flatsawn board still loses 2.2 times the width of a quartersawn one.
0.32 in.
off a 6-inch flatsawn board, green to oven-dry; quartersawn 0.14 in.
- Tangential
- 5.3%
- Radial
- 2.4%
- Volume
- 8.9%
- T/R ratio
- 2.21 (131st most stable of 155)
End view, shrinkage drawn 3× life size.
Closest substitutes
- Hura
13% softer · 5% lighter · shrinks 0.8 points less across the face
- Primavera
5% harder · same density · shrinks 0.2 points less across the face
- African mahogany
32% harder · 5% heavier · shrinks 0.8 points less across the face
Woods of similar hardness
The eight nearest on the Janka scale, lbf.
Laboratory values
Its most unusual laboratory figure is crushing strength along the grain: 6th lowest of the 154 woods with a published value.
| Property | Green | Dry, 12% MC | Change when dried | Metric, 12% MC |
|---|---|---|---|---|
| Compression parallel to grain | 2,460psi | 4,290psi | +74% | 29.6MPa |
| Modulus of elasticity | 0.94M psi | 1.11M psi | +18% | 7.65GPa |
| Modulus of rupture | 5,900psi | 8,600psi | +46% | 59.3MPa |
| Shear parallel to grain | 860psi | 1,060psi | +23% | 7.30MPa |
| Work to maximum load | 5.40in-lbf/in³ | 7.20in-lbf/in³ | +33% | 49.6kJ/m³ |
| Side hardness | 440lbf | 630lbf | +43% | 2,802N |
Wood Handbook Table 5-5b, Table 4-4. Data & method · Guides