Guibourtia arnoldiana
Benge measures 1,750 lbf on the Janka scale, 36% harder than northern red oak.
U.S. hardwoodsU.S. softwoodsImported woodsNorthern red oak
Six measures
BengeImported woods medianOther woods
Bending strength
21,400 psi147.5 MPa13th strongest of 15528% above the imported woods median4,300 psi29,900 psiJanka hardness
1,750 lbf7,784 N25th hardest of 15521st of 65 imported woods; 35% above the imported woods median240 lbf3,680 lbfDensity
0.6528th heaviest of 1550.250.96Stiffness
2.04 M psi14.1 GPa36th stiffest of 1550.54 M psi4.06 M psiCupping tendency
1.6549th lowest of 1551.092.90Shrinkage across the face
8.6%radial 5.2%52nd highest of 1553.5%12.7%
For its weight: strength-to-weight 32,923 psi (3rd of 155).
How much it moves
Both its face shrinkage (8.6%) and its T/R ratio (1.65) sit in the middle half of the list.
0.52 in.
off a 6-inch flatsawn board, green to oven-dry; quartersawn 0.31 in.
- Tangential
- 8.6%
- Radial
- 5.2%
- Volume
- 13.8%
- T/R ratio
- 1.65 (49th most stable of 155)
End view, shrinkage drawn 3× life size.
Closest substitutes
- Degame
11% harder · 3% heavier · same face shrinkage
- Courbaril
34% harder · 9% heavier · shrinks 0.1 points less across the face
- Black locust
3% softer · 2% heavier · shrinks 1.4 points less across the face
Woods of similar hardness
The eight nearest on the Janka scale, lbf.
Laboratory values
Its most unusual laboratory figure is crushing strength along the grain: 10th highest of the 154 woods with a published value.
| Property | Dry, 12% MC | Metric, 12% MC |
|---|---|---|
| Compression parallel to grain | 11,400psi | 78.6MPa |
| Modulus of rupture | 21,400psi | 147.5MPa |
| Shear parallel to grain | 2,090psi | 14.4MPa |
| Side hardness | 1,750lbf | 7,784N |
| Modulus of elasticity | 2.04M psi | 14.1GPa |
The handbook publishes only values at 12% moisture content for this wood; green values and some tests are not given.
Wood Handbook Table 5-5b, Table 4-4. Data & method · Guides