Chestnut oak
Quercus prinus
Chestnut oak measures 1,130 lbf on the Janka scale, 12% softer than northern red oak.
- It is softer than its weight suggests: the trend across all 155 woods puts a specific gravity of 0.57 near 1,380 lbf.
- Andiroba has exactly the same Janka figure.
- Overall it falls in the top fifth for face shrinkage, radial shrinkage and volumetric shrinkage.
U.S. hardwoodsU.S. softwoodsImported woodsNorthern red oak
Six measures
Chestnut oakU.S. hardwoods medianOther woods
Shrinkage across the face
10.8%radial 5.3%15th highest of 1553.5%12.7%Cupping tendency
2.0442nd highest of 1551.092.90Density
0.570.66 at 12% MC49th heaviest of 1550.250.96Stiffness
1.59 M psi11.0 GPa66th most flexible of 1550.54 M psi4.06 M psiJanka hardness
1,130 lbf5,026 N67th hardest of 15528th of 53 U.S. hardwoods240 lbf3,680 lbfBending strength
13,300 psi91.7 MPa70th strongest of 1554,300 psi29,900 psi
How much it moves
Its face shrinkage of 10.8% is in the top quarter of the list, with an ordinary T/R ratio of 2.04.
0.65 in.
off a 6-inch flatsawn board, green to oven-dry; quartersawn 0.32 in.
- Tangential
- 10.8%
- Radial
- 5.3%
- Volume
- 16.4%
- T/R ratio
- 2.04 (114th most stable of 155)
End view, shrinkage drawn 3× life size.
Closest substitutes
- Swamp chestnut oak
10% harder · 5% heavier · same face shrinkage
- Post oak
20% harder · 5% heavier · shrinks 1.0 points less across the face
- White oak
20% harder · 5% heavier · shrinks 0.3 points less across the face
Among the oaks
14th hardest of 15, lbf; the neighbours either side are shown, the rest are on the oaks page.
Laboratory values
| Property | Green | Dry, 12% MC | Change when dried | Metric, 12% MC |
|---|---|---|---|---|
| Impact bending | 35in. | 40in. | +14% | 1,016mm |
| Compression perpendicular | 530psi | 840psi | +58% | 5.80MPa |
| Modulus of elasticity | 1.37M psi | 1.59M psi | +16% | 11.0GPa |
| Side hardness | 890lbf | 1,130lbf | +27% | 5,026N |
| Modulus of rupture | 8,000psi | 13,300psi | +66% | 91.7MPa |
| Shear parallel to grain | 1,210psi | 1,490psi | +23% | 10.3MPa |
| Work to maximum load | 9.40in-lbf/in³ | 11in-lbf/in³ | +17% | 75.8kJ/m³ |
| Compression parallel to grain | 3,520psi | 6,830psi | +94% | 47.1MPa |
| Tension perpendicular | 690psi | not tested | — | — |
Wood Handbook Table 5-3b, Table 4-3. Data & method · Guides